Description
ASTM E372 – Standard Test Method for Determination of Calcium and Magnesium in Magnesium Ferrosilicon by EDTA Titrimetry
1.1”This test method covers the chemical analysis of magnesium ferrosilicon having chemical compositions within the following limits:
Element |
Composition Range,”’% |
” |
|
Aluminum |
2.0 max |
Calcium |
0.25 to 3.00 |
Carbon |
0.50 max |
Cerium |
1.0 max |
Chromium |
0.50 max |
Magnesium |
2.00 to 12.00 |
Manganese |
1.0 max |
Silicon |
40.00 to 55.00 |
Sulfur |
0.025 max |
Titanium |
0.2 max |